Zum Hauptinhalt springen
Nicht aus der Schweiz? Besuchen Sie lehmanns.de
Precision Forming Technology of Large Superalloy Castings for Aircraft Engines - Baode Sun, Jun Wang, Da Shu

Precision Forming Technology of Large Superalloy Castings for Aircraft Engines (eBook)

, , (Autoren)

eBook Download: PDF
2021
XI, 410 Seiten
Springer Singapore (Verlag)
978-981-336-220-8 (ISBN)
Systemvoraussetzungen
181,89 inkl. MwSt
(CHF 177,70)
Der eBook-Verkauf erfolgt durch die Lehmanns Media GmbH (Berlin) zum Preis in Euro inkl. MwSt.
  • Download sofort lieferbar
  • Zahlungsarten anzeigen

This book describes systematically the theory and technology of the precision forming of large, complex and thin-walled superalloy castings for aircraft engines, covering all the important basic aspects of the manufacturing process, including process design, wax pattern, ceramic molds, casting and solidification, heat treatment, repair casting and dimension precision control.

The correlation of casting defects, structural characteristics and performance of castings is revealed through a range of tests. It also discusses the latest technologies and advances in this field - such as imaging the solidification process by means of synchrotron radiography, 3D computerized tomography and reconstruction of microporosity defects, analysis and diagnosis of error sources for dimension over-tolerance and adjusted pressure casting technology - which are of particular interest. Providing essential insights, the book offers a valuable guide to the design and manufacture of superalloy casting parts for aircraft engines.




Baode Sun is Chair Professor of Materials Science and Engineering at Shanghai Jiao Tong University (SJTU). He received his Ph.D. degree from Northwestern Polytechnic University, China, in 1993. He became 'Yangtze River Scholar' Distinguished Professor in 2007 and Dean of School of Materials Science and Engineering in 2013. His research is focused on the fundamental and applied aspects of liquid metal processing and investment casting of large-size thin-wall structural components. He has published more than 200 technical papers, and he holds more than 100 Chinese patents. He won numerous prestigious research awards, such as the second prize of the National Technology Invention Award of China and the first prize of the Shanghai Science and Technology Invention Award.

Jun Wang is Professor of Materials Processing at SJTU. He received his B.Sc. (1991), M.Sc. (1994) and Ph.D. (1997) at Southeast University. He was Research Fellow in the Venture Business Lab in Saga University and Senior Researcher in the Department of Materials Engineering at the University of Tokyo in Japan. His research focuses on investment casting process. He has published more than 200 peer-reviewed articles, and he holds 95 China patents and one US patent. He received a number of awards, including the 2nd prize of the National Technology Invention Award, the New Century Talents of Ministry of Education, China, and Shanghai Excellent Scientific Leader. 

Da Shu is Professor of Materials Processing at SJTU. He received his B.Sc. (1994) at Nanjing University of Aeronautics and Astronautics and his M.Sc. (1997) and Ph.D. (2001) at SJTU. He was Academic Visitor at the Department of Materials, Oxford University, in 2009-2010. His research focuses on processing of advanced metallic materials and control of solidified structure. He has published more than 100 peer-reviewed articles, and he holds 30 China patents and one US patent. He received a number of awards, including the 2nd prize of the National Technology Invention Award, Rising-Star of Shanghai Municipal Science and Technology Commission and the New Century Talents of Ministry of Education, China.


This book describes systematically the theory and technology of the precision forming of large, complex and thin-walled superalloy castings for aircraft engines, covering all the important basic aspects of the manufacturing process, including process design, wax pattern, ceramic molds, casting and solidification, heat treatment, repair casting and dimension precision control.The correlation of casting defects, structural characteristics and performance of castings is revealed through a range of tests. It also discusses the latest technologies and advances in this field such as imaging the solidification process by means of synchrotron radiography, 3D computerized tomography and reconstruction of microporosity defects, analysis and diagnosis of error sources for dimension over-tolerance and adjusted pressure casting technology which are of particular interest. Providing essential insights, the book offers a valuable guide to the design and manufacture of superalloy casting parts for aircraft engines.
Erscheint lt. Verlag 6.2.2021
Zusatzinfo XI, 410 p. 269 illus., 131 illus. in color.
Sprache englisch
Themenwelt Technik Elektrotechnik / Energietechnik
Technik Fahrzeugbau / Schiffbau
Technik Luft- / Raumfahrttechnik
Technik Maschinenbau
Schlagworte Adjusted Pressure Casting • Ceramic Shell • Dimension Over-tolerance • Gating and Riser System • Investment Casting • Precision Forming • Solidification Defects • Solidification Structure • Superalloy Casting • Wax Pattern
ISBN-10 981-336-220-0 / 9813362200
ISBN-13 978-981-336-220-8 / 9789813362208
Informationen gemäß Produktsicherheitsverordnung (GPSR)
Haben Sie eine Frage zum Produkt?
PDFPDF (Wasserzeichen)

DRM: Digitales Wasserzeichen
Dieses eBook enthält ein digitales Wasser­zeichen und ist damit für Sie persona­lisiert. Bei einer missbräuch­lichen Weiter­gabe des eBooks an Dritte ist eine Rück­ver­folgung an die Quelle möglich.

Dateiformat: PDF (Portable Document Format)
Mit einem festen Seiten­layout eignet sich die PDF besonders für Fach­bücher mit Spalten, Tabellen und Abbild­ungen. Eine PDF kann auf fast allen Geräten ange­zeigt werden, ist aber für kleine Displays (Smart­phone, eReader) nur einge­schränkt geeignet.

Systemvoraussetzungen:
PC/Mac: Mit einem PC oder Mac können Sie dieses eBook lesen. Sie benötigen dafür einen PDF-Viewer - z.B. den Adobe Reader oder Adobe Digital Editions.
eReader: Dieses eBook kann mit (fast) allen eBook-Readern gelesen werden. Mit dem amazon-Kindle ist es aber nicht kompatibel.
Smartphone/Tablet: Egal ob Apple oder Android, dieses eBook können Sie lesen. Sie benötigen dafür einen PDF-Viewer - z.B. die kostenlose Adobe Digital Editions-App.

Buying eBooks from abroad
For tax law reasons we can sell eBooks just within Germany and Switzerland. Regrettably we cannot fulfill eBook-orders from other countries.

Mehr entdecken
aus dem Bereich
Kommunikationssysteme mit EIB/KNX, LON, BACnet und Funk

von Thomas Hansemann; Christof Hübner; Kay Böhnke

eBook Download (2025)
Hanser (Verlag)
CHF 38,95
Verfahren zur Berechnung elektrischer Energieversorgungsnetze

von Karl Friedrich Schäfer

eBook Download (2023)
Springer Fachmedien Wiesbaden (Verlag)
CHF 107,45