Metallography and Fractography XVII
Trans Tech Publications Ltd (Verlag)
9783035716122 (ISBN)
Selected, peer-reviewed papers from the 17th International Symposium on Metallography, Fractography and Materials Science (Metallography XVII), April 24 – 26, 2019, Nový Smokovec, High Tatra Mountains, Slovak Republic
This volume contains selected papers presented at the
17th International Symposium on Metallography, Fractography and Materials Science (April 24 – 26, 2019, Nový Smokovec, High Tatra Mountains, Slovak Republic). Collected articles focus on not only research in the field of steel, alloys, and metallic materials but also in the field of numerous modern materials and technologies - ceramics, composites, amorphous materials, special coatings, and powder metallurgy.
Preface
Invited Lectures
Boronizing of AISI 316L Stainless Steel Using Spark Plasma Sintering Technique
Novel Cost-Efficient Method of Producing Ausferritic Steels Displaying Excellent Combination of Mechanical Properties
The Copper-Arsenic Eutectic and the Cu3As Phase
Metallographic Documentation of the Degradation of Iron and Nickel Based Alloys in HCl and H2S Containing Environments, between 480 – 680 °C
Characterisation of Chemical Vapour Deposited AlHfN Coatings
Chapter 1: Process Simulation and Metallographic Methods
The Influence of Surface Dipping and Bulk Filling Agents on Properties of High-Speed Grinding Wheels: Materialographic-Based Numerical Modelling
A Thermomechanical Model of Retention of a Diamond Particle in Matrices Based on Fe
Investigation of the Diffusion Couple Ductile Cast Iron / Iron
SEM Imaging of In Situ Tensile Testing of 27CrNiMoV Steel
Nanomechanical Characterization of Iron Borides in Fe-Mn-B Ternary Alloys
Chapter 2: Solidification and Solid State Transformation
Simultaneous Fabrication of Multiple Castings Using Frozen Mold Casting Method
The Effect of Heat-Treatment on the Phase Stability of Fe-28Al-15Si-2Mo Alloy
The Microstructure Evolution of Fe-28Al-15Si-0.2Zr Alloy during Different Heat-Treatment
Structural Nature of ZnAl4Cu1 Alloy Plasticity Affected by Various Technological Treatments
Microstructural and Fractographic Analysis of CuAlNi Shape Memory Alloy before and after Heat Treatment
Chapter 3: Interrelationship between Microstructure and Material Properties
Inclusion Engineering in Structural Steels with Enhanced Machinability
Texture Evolution during Cold Drawing of Steel Tube with Respect to the Stress - Strain State
Microstructure Influenced by Controlled Rolling, Cooling and Thermal Processing of Seamless Tubes Made of Steel 25CrMo4
Microstructure, Substructure and Mechanical Properties of 9CrNB Steel after Tempering
Comparison of Microstructure and Mechanical Properties of Additively Manufactured and Conventional Maraging Steel
Structure and Properties of Bakelite Bonded Grinding Wheels
The Influence of Secondary Phase on Impact Toughness of Alloyed Iron Aluminides
Biodegradable Iron-Based Foams for Potential Bone Replacement Material
Chapter 4: Welding
On the Surface Welding of Pearlitic Rails: The Control of Dilution and Microstructure
Analysis of the Cause of Damage to the Steam Generator Cold Collector’s Dissimilar Weld Joint at Slovak Nuclear Power Plant
Possibilities for Using New Types of Additive Materials for Hardfacing
Analysis of Causes of Baby Stroller Construction Damage
Chapter 5: Fractures, Defects and Material Degradation
Fractography of Additively Manufactured Titanium Alloy: Influence of Post-Processing Treatment
Influence of Boric Acid Solution and Gamma Irradiation on Selective Sorbents
Surface Chemistry-Based Surface Defects Situated on Steel Strips Edges
The Failure of Carbon Fiber Reinforced Composite Analyzed by Acoustic Emission
Size Effect in Plastic Deformation and Failure of Metallic Glasses
Analysis of Causes of Defects Appearance in Wire Drawing
Metallographic Analysis of Stainless Steel Inner Shaft of Centrifugal Pump
Investigation of Screw Failed During Installation
Rarely Occurring Defects on Tinplates
Defects of Steel Sheets Joined by Laser Welding
Analysis of Corrosion Resistance of Heat Exchanger Plates Made of AISI 316L Steel
Microstructural and Chemical Analysis of Military Steel from World War II as Part of Sculpture
Chapter 6: Fatigue and Creep
3D Textural Analysis of Fatigue Fracture Surfaces
Character of Fatigue Damage under Axial, Torsional and Biaxial Loading of 316L Stainless Steel
The Effect of Prior Surface Roughness on Fatigue Life of Nitrided Specimens
Detection of Early Stage of Fatigue Changes in Non-Alloy Steel Using Residual Magnetic Field Method
Estimating of the Size of the Maximum Non-Metallic Inclusions in Martensitic Steels and their Influence on Fatigue Properties
The SEM and TEM Analysis of IN718 Alloy after Fatigue Push-Pull Loading at 700°C
Characterization of Microstructure of Crept Samples of Dissimilar Weld Joint Using Standard and Advanced Electron Microscopy Techniques
Evaluation of Cavitation Damage in a Pipe Bend Made of 0.5Cr-0.5Mo-0.3V Steel by Optical Metallography and Replica Method
Near-Surface Structure and Fatigue Crack Initiation Mechanisms of As-Built SLM Inconel 718
Fatigue Behavior of Titanium Endoprosthesis
Influence of Cyclic Loading on the Internal Friction Measured on Magnesium Alloys AZ31, AZ61 and AZ91
SnO2 Nano/Microfibers for Gas Sensors
Chapter 7: Nonferrous Alloys
Effects on Microstructure and Corrosion Behavior of a Heat Treated CuZn36Pb2 Brass
Small Scale Plastic Yielding of Mg Alloys Assessed with Nanoindentation
Magnesium Alloy WE43 Produced by 3D Printing (SLM)
Experimental Verification of Phase Diagram Calculations of Zr-Based Alloys after High-Temperature Oxidation
Consequences of Inappropriate Temperatures of the Solution Heat Treatment in Al-Si-Cu Cast Alloys
Characterization of High-Speed Alumina Abrasive Grinding Wheel
Chapter 8: Powder Metallurgy
Step-Sintering of Fe-(1-3)%Mn-0.8%C Steels
Microstructure and Mechanical Properties of Fe-Cu-Ni Sinters Prepared by Ball Milling and Hot Pressing
Characterization of Mg-Zn Layered Bulk Materials Prepared by Powder Metallurgy Method
Influence of Oxide Dispersoids on the Structure Development of Copper Nanocomposite Prepared by Spark Plasma Sintering Technology
Preparation of Cerium Stabilized Zirconia Bulk Ceramics by Spark Plasma Sintering
Sintering of High Mn Cemented Carbides in Mn-Rich Environment
Chapter 9: Surface Engineering and Coatings
Microstructure, Stiffness and Corrosion of Bare and Phosphated Specimens Made by Sintering of Structured Iron-Iron Oxide Spheres
Thermal Cyclic Behaviour of Conventional YSZ and Mullite-YSZ Thermal Barrier Coatings
Influence of RF Plasma Jet Surface Treatment on Wetting Behavior of Yttria Stabilized Zirconia SPS Coatings
Microstructure Characteristics, Tribology and Nano-Hardness of Plasma Sprayed NiCrRe Coating
Microstructure Characteristics, Tribology and Nano-Hardness of HVOF Sprayed NiCrRe Coating
Anodizing of Pure Magnesium in Sodium Hydroxide Electrolyte Solution
| Erscheinungsdatum | 16.01.2021 |
|---|---|
| Reihe/Serie | Defect and Diffusion Forum |
| Zusatzinfo | Illustrations |
| Verlagsort | Zurich |
| Sprache | englisch |
| Maße | 170 x 240 mm |
| Gewicht | 930 g |
| Themenwelt | Naturwissenschaften ► Physik / Astronomie ► Mechanik |
| Technik ► Maschinenbau | |
| ISBN-13 | 9783035716122 / 9783035716122 |
| Zustand | Neuware |
| Informationen gemäß Produktsicherheitsverordnung (GPSR) | |
| Haben Sie eine Frage zum Produkt? |
aus dem Bereich